Show simple item record

dc.contributor.authorAdıgüzel, Mehmet
dc.contributor.authorÖztekin, Faruk
dc.date.accessioned2021-09-03T11:37:44Z
dc.date.available2021-09-03T11:37:44Z
dc.date.issued2020en_US
dc.identifier.citationADIGÜZEL M,ÖZTEKİN F (2020). Comparison of the resistance to cyclic fatigue of One Curve, One Shape, 2Shape and EdgeFile X3 files in simulated single and S-shaped (double) curvatures. International Dental Research, 10(2), 55 - 59.en_US
dc.identifier.issn2146-1767
dc.identifier.urihttps://dx.doi.org/10.5577/intdentres.2020.vol10.no2.5
dc.identifier.urihttps://hdl.handle.net/20.500.12483/3305
dc.description.abstractAim: To evaluate the fracture resistance to cyclic fatigue of One Curve (Micro Mega, Besancon, Cedex, France), One Shape (Micro-Mega), 2Shape (Micro-Mega) and EdgeFile X3 (EdgeEndo, Albuquerque, NM) files in simulated root canals. Methodology: One hundred and sixty nickel-titanium endodontic files were tested in simulated canals with single and s-shaped (double) curvatures. The One Curve (25/.06), One Shape (25/.06), 2Shape (25/.06) and EdgeFile X3 (25/.06) files were assessed (n=20 for each test). All the files were rotated up to fracture occurred. The number of cycles to fracture (NCF) was determined and also, the length of the fractured file part was measured. For statistical analysis, one-way analysis of variance and Tukey HSD tests were used (p < 0.05). Results: NCF for all instrument groups were significantly higher in the single curvature canal compared to the s-shaped curvature canal (p < 0.05). The EdgeFile X3 had the highest fatigue resistance in both curvature groups. The NCF of the One Curve were higher than that of the One Shape and 2Shape files (P < 0.05). In the s-shaped curvature canal, the files inclined to fracture more often in the apical curvature compared to the coronal curvature. There was no statistically considerable difference in the length of the fractured parts among the four experiment groups in either the single or s-shaped canal curvatures (p > 0.05). Conclusion: Within the limitations of this study, fracture resistance to cyclic fatigue was the highest for the EdgeFile X3 group followed by the One Curve group and lowest for the 2Shape and One Shape group.en_US
dc.language.isoengen_US
dc.publisherDicle Üniversitesien_US
dc.relation.isversionof10.5577/intdentres.2020.vol10.no2.5en_US
dc.rightsinfo:eu-repo/semantics/openAccessen_US
dc.subject2Shapeen_US
dc.subjectCyclic fatigueen_US
dc.subjectEdgeFile X3en_US
dc.subjectOne Curveen_US
dc.subjectOne Shapeen_US
dc.titleComparison of the resistance to cyclic fatigue of One Curve, One Shape, 2Shape and EdgeFile X3 files in simulated single and S-shaped (double) curvaturesen_US
dc.typearticleen_US
dc.relation.journalInternational Dental Researchen_US
dc.contributor.departmentDiş Hekimliği Fakültesien_US
dc.contributor.authorID0000-0002-9363-6264en_US
dc.identifier.volume10en_US
dc.identifier.issue2en_US
dc.identifier.startpage55en_US
dc.identifier.endpage59en_US
dc.relation.publicationcategoryMakale - Ulusal Hakemli Dergi - Kurum Öğretim Elemanıen_US


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record